Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | |
NHEP Spectron™ E5469 Nylon 66, 33% Glass Fiber Natural color. E5469 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informat.. |
|||
Front Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 255°C |
Kingfa PA66-ROW Halogen-free, Flame Retardant PA66 Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingConnectors, linkersRelay, bobbins, plugsHousehold appliance parts.. |
|||
Front Barrel Temperature | 240 - 265 °C | 464 - 509 °F | Start Point: 255°C |
Kingfa PBT-RG152 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S.. |
|||
Front Barrel Temperature | 240 - 265 °C | 464 - 509 °F | Start Point: 255°C |
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Front Barrel Temperature | 240 - 265 °C | 464 - 509 °F | Start Point: 255°C |
Kingfa PBT-RG301 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingHousehold appliance partsBobbinLighting partsRelayLinkerInformati.. |
|||
Front Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 255°C |
Kingfa UTPBT-HB Toughened PBT Features:High impactExcellent size stabilityEasy processingApplications:Injection moldingSwitch partsKeyboard keysE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 240 - 265 °C | 464 - 509 °F | Injection Molding |
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® SG5152 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good Surface, High ImpactApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® TE5000LZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provide.. |
|||
Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® TE5000S PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided.. |
|||
Front Barrel Temperature | 245 - 265 °C | 473 - 509 °F | |
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5100 PC/ABS+GF10% Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
Front Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY HI5002A PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® TE5000GH PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Garnish)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |