Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 330 - 360 °C | 626 - 680 °F | |
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Front Barrel Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika P-3001S Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Front Barrel Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
Front Barrel Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |