Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ Electro 242-0 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ Electro 242-15 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ Electro 940 Liquid Silicone Rubber - Medium Voltage This LSR elastomer is a medium voltage, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperat.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ FFSL 7286/40 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2530 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2631 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2645 Custom Liquid Silicone Rubber - Infant Care This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2660 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2750 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 2760 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/60 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 3485/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 4020 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 4660 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 4670 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 7005 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 3386/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Siloprenâ„¢ LSR 4080 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Nozzle Temperature | 20.0 °C | 68.0 °F | cool nozzle and cylinder to prevent premature vulcanization |
Momentive Performance Materials Silopren™ LSR 3386/30 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |