Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika L-1003PA Heat resistance, creep resistance, and excellent lubricantInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika P-1001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |