Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P251-01 Polypropylene Copolymer, Black Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Nozzle Temperature | 199 - 216 °C | 390 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Nozzle Temperature | 199 - 216 °C | 390 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC SunPro® SP 200 P4058 Polypropylene Copolymer SunPro® SP 200 P 4058 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: Chrysl.. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer X-PRO PP 2015 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2040 Polypropylene Copolymer X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO PP 2021 Polypropylene Impact Copolymer X-PRO PP 2021 is an impact, polypropylene copolymer. It has general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | Average value: 210 °C Grade Count:3 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |