Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 3018 TU Polypropylene Talc Filled, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 4008 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 4009 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 4012 TH Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products FT4650-01UV Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products FT5100-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products HP532-01 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: Close out panelSpeaker grilleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products T20P105-00FA 20% Talc Reinforced Polypropylene, FDA Compliant Components, Natural Applications: Food traysFood service implementsContainersConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 227 °C | 410 - 440 °F | |
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |