Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 220 - 270 °C | 428 - 518 °F | |
Ovation Polymers Nemcon™ H ABS DP116P ABS ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | Average value: 255 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Nozzle Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Nozzle Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000G PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 24968-12-5 and 103598-77-2Information provid.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000LZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provide.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6 Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? G.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika AXF-1500-05 Conditioned Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika U-8400H U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 200 - 270 °C | 392 - 518 °F | |
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Nozzle Temperature | 200 - 270 °C | 392 - 518 °F | |
Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN301-G35 Nylon 66 Resin 35% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |