Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 110 °C | 230 °F | optimum |
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**) Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a.. |
|||
Mold Temperature | 110 °C | 230 °F | optimum |
DuPont Performance Polymers Rynite® 940 NC010 PET
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 110 °C | 230 °F | optimum |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
Mold Temperature | 110 °C | 230 °F | optimum |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 110 - 150 °C | 230 - 302 °F | |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Mold Temperature | 110 °C | 230 °F | for test specimens; ISO 294 |
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Mold Temperature | 110 °C | 230 °F | for test specimens; ISO 294 |
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Mold Temperature | 110 °C | 230 °F | |
Toyobo ECOVYLOPET® EMC2310 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | actual surface temp |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | |
Covestro Apec® 1703 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable .. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® GF9002* Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-18-9,GF10Formerly Makrolon DP1-1889MVR (300 °C/1.2 kg) 15 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.2 mmUL 94 5VA/2.8 mm (Bayer .. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection molding; ISO 294 |
Covestro Makrolon® SF810 Polycarbonate, Glass Fiber Reinforced Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Structural foam• 10%.. |
|||
Mold Temperature | 110 - 129 °C | 230 - 265 °F | |
Entec Hylex® P1302B Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® DP1-1888* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-09-3,GF20Developmental productMVR (300 °C/1.2 kg) 10 cm3/10 min20 % Glass fiber reinforcedMilled fiberMedium viscosityEasy releasegood surface qualityInjection molding - Melt te.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection Molding; ISO 10724 |
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 8.0 cm3/10 minStructural foam5 % Glass fiber reinforcedMilled fiberChlorine- and bromine-free flame retardantMedium viscosityEasy releaseInjection moldingAvailable in natural (o.. |
|||
Mold Temperature | 110 °C | 230 °F | Injection molding |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | actual surface temp |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Mold Temperature | 110 °C | 230 °F | optimum |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
Mold Temperature | 110 °C | 230 °F | optimum |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |