Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 121 °C | 250 °F | |
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC) Information provided by PolyOne |
|||
Mold Temperature | 121 °C | 250 °F | |
PolyOne Edgetek® PS-30GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued ** Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Lubricomp® EFL-4036 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Stat-Kon® EC-1004 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® EC-1006 EM Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® EF-1004 BK8-115 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Lubri-Tech™ PF-30CF/15T Polysulfone, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 121 - 163 °C | 250 - 325 °F | |
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)
(discontinued **) Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that.. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Edgetek® SF-30GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Therma-Tech™ SF-5000C TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Mold Temperature | 121 - 163 °C | 250 - 325 °F | |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Mold Temperature | 121 - 163 °C | 250 - 325 °F | |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Mold Temperature | 121 - 177 °C | 250 - 350 °F | |
PolyOne Lubri-Tech™ PI-000/15T Polyetherimide (PEI), PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade Data provided by PolyOne. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Mold Temperature | >= 121 °C | >= 250 °F | |
PolyOne Lubri-Tech™ MP-20GF/05T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 121 °C | 250 °F | |
PolyOne Lubri-Tech™ MP-000/15T Modified PPO - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 121 °C | 250 °F | |
PolyOne Lubri-Tech™ MP-30GF/15T Modified PPO - 30% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |