Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 18.0 - 71.0 °C | 64.4 - 160 °F | |
Albis Plastics Polypropylene A 12 H-GK20/GF20 C , 20% Glass Bead/20% Glass Fiber
(discontinued **) Semi-crystalline Polypropylene Homopolymer (PPHP)Characteristics: Chemically Coupled Fiber; Good Dimensional StabilityApplications: Appliances, Furniture, Cases, Packaging and NoveltiesProcessing: I.. |
|||
Mold Temperature | 18.0 - 75.0 °C | 64.4 - 167 °F | |
Lavergne VYPET VNT 1020 Polyester-PC Alloy The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Mold Temperature | 18.0 - 75.0 °C | 64.4 - 167 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Mold Temperature | 18.0 - 71.0 °C | 64.4 - 160 °F | Average value: 46.9 °C Grade Count:8 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Mold Temperature | 18.0 - 80.0 °C | 64.4 - 176 °F | Average value: 51.0 °C Grade Count:95 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |