Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Bergamid™ A70 G5 T Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Mold Temperature | 62.8 - 85.0 °C | 145 - 185 °F | Average value: 73.9 °C Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Mold Temperature | 60.0 - 85.0 °C | 140 - 185 °F | Injection Molding |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Mold Temperature | 60.0 - 85.0 °C | 140 - 185 °F | |
LATI Latiohm 75/4-10 CNT PBT Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Mold Temperature | 57.2 - 85.0 °C | 135 - 185 °F | |
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 60.0 - 85.0 °C | 140 - 185 °F | |
BASF Ultramid® BU50I BK 106 PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I BK-106 is an unreinforced PA6, impact modified, pigmented black, injection molding product that maintains its impact strength and ductility to -40 deg F .. |