Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 21.1 - 100 °C | 70.0 - 212 °F | Average value: 59.6 °C Grade Count:26 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal
(Unverified Data**) Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such.. |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | DAM |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | Injection Molding |
LG Chemical Lupox® HI2100M PBT+GF10% Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latilub 87/28-20T PC, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE.Information provided by Lati Industria Termoplastici S.p.A. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
E-Polymers TEKAPPO® J910 10% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
E-Polymers TEKAPPO® JF6 Un-Reinforced Flame Retardant Heat Resistance M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
BASF Ultradur S 4090 G4 High Speed Unc. 20% Glass Filled PBT Ultradur S 4090 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |