Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 27.0 - 60.0 °C | 80.6 - 140 °F | |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Mold Temperature | 27.0 - 60.0 °C | 80.6 - 140 °F | |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Mold Temperature | 27.0 °C | 80.6 °F | |
Eastman Eastar Copolyester K3000 PETG Copolyester
(discontinued **) EASTAR K3000 Copolyester is a cost effective, high-performance, water-clear material that provides the necessary performance for the appliance standards. Other desirable characteristics are good ch.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarityEnhanced mold releaseGood elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilization Applications: DisplaysMedical devicesOffice acc.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer
(discontinued **) Features: High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationExcellent indoor light stabilityHigh elongation and ductilityApplications: Appliance.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class .. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiationApplications: Display, medical de.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 8077 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 27.0 - 49.0 °C | 80.6 - 120 °F | |
PolyOne Edgetek® AS-1000 SD Unreinforced ABS - Antistatic Protection
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
PolyOne Edgetek® AS-10CF/000 ABS - 10% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Mold Temperature | 27.0 - 49.0 °C | 80.6 - 120 °F | |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Mold Temperature | 27.0 - 49.0 °C | 80.6 - 120 °F | |
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer .. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Mold Temperature | 27.0 - 107 °C | 80.6 - 225 °F | Average value: 61.1 °C Grade Count:39 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection.. |