Processing Properties Metric English Comments
Mold Temperature 190 - 220 °C
374 - 428 °F
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Mold Temperature 190 - 210 °C
374 - 410 °F
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Mold Temperature 190 - 200 °C
374 - 392 °F
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Mold Temperature 190 - 215 °C
374 - 419 °F
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Mold Temperature 190 - 215 °C
374 - 419 °F
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
Mold Temperature 190 - 215 °C
374 - 419 °F
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Mold Temperature 190 - 215 °C
374 - 419 °F
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of ..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..