Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | |
Albis Plastics PC/PET 361E Unfilled
(discontinued **) Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and.. |
|||
Mold Temperature | 49.0 - 71.0 °C | 120 - 160 °F | |
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 60.0 - 71.0 °C | 140 - 160 °F | |
PolyOne Lubri-Tech™ ATH-000/02T Homopolymer - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 18.0 - 71.0 °C | 64.4 - 160 °F | |
Albis Plastics Polypropylene A 12 H-GK20/GF20 C , 20% Glass Bead/20% Glass Fiber
(discontinued **) Semi-crystalline Polypropylene Homopolymer (PPHP)Characteristics: Chemically Coupled Fiber; Good Dimensional StabilityApplications: Appliances, Furniture, Cases, Packaging and NoveltiesProcessing: I.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | |
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 38.0 - 71.0 °C | 100 - 160 °F | Average value: 54.4 °C Grade Count:7 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Mold Temperature | 18.0 - 71.0 °C | 64.4 - 160 °F | Average value: 46.9 °C Grade Count:8 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |