Processing Properties Metric English Comments
Rear Barrel Temperature 205 °C
401 °F
Multibase Nylex™ 1230 Natural Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Rear Barrel Temperature 205 °C
401 °F
Multibase Nylex™ 1404 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Rear Barrel Temperature 205 °C
401 °F
Multibase Nylex™ 2185 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Rear Barrel Temperature 205 °C
401 °F
Multibase Nylex™ 2185 R15 Polyamide + PP
Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho..
Rear Barrel Temperature 205 °C
401 °F
Multibase Nylex™ 2185 R30 Polyamide + PP
Glass fiber reinforcement, 30% Filler by Weight Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Method..
Rear Barrel Temperature 205 °C
401 °F
Multibase TPSiV™ 3011-85A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
Rear Barrel Temperature 205 °C
401 °F
Multibase Nylex™ 2185 FR Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..
Rear Barrel Temperature 205 - 225 °C
401 - 437 °F
Injection Molding
LG Chemical KEYFLEX BT 1245D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Medium Modulus, Black colorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
Rear Barrel Temperature 205 - 235 °C
401 - 455 °F
Injection Molding
LG Chemical KEYFLEX BT 3038D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Rear Barrel Temperature 205 °C
401 °F
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..
Rear Barrel Temperature 205 °C
401 °F
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF
A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Rear Barrel Temperature 205 °C
401 °F
Injection
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer
Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 205 °C
401 °F
Injection
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 205 °C
401 °F
Injection
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..