Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | |
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo.. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Start Point: 215°C |
Kingfa JE2-R2 ABS/PBT Alloy Features:Low costExcellent balance propertiesGood processing propertiesGood heat stabilityGood size stabilityGood surfaceApplications:CD-ROM, DVDPrinter, scanner, photocopier cabinetElectric and ele.. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Start Point: 215°C |
Kingfa JH950-402 Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a.. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Start Point: 230°C |
Kingfa MAC-301 PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel.. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical KEYFLEX BT HB9242D Ester Type TPE Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Rear Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOY GN-5001TF Halogen Free PC/ABS Alloy, High Flow, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay Technyl® C 206 Nylon 6, EH0 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay Technyl® C 206 Nylon 6, EH50 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Rear Barrel Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Rear Barrel Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Unitika AXF-1500-05 Conditioned Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Unitika AXF-1500-05 Dry Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Zone 1 |
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Zone 1 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Rear Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Pipe Extrusion |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Rear Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |