Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 230 - 255 °C | 446 - 491 °F | Start Point: 235°C |
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Rear Barrel Temperature | 230 - 255 °C | 446 - 491 °F | Start Point: 235°C |
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Start Point: 245°C |
Kingfa PET-RG20 Flame Retardant, 20% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Start Point: 245°C |
Kingfa PET-RG30 Flame Retardant, 30% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Industrial MaterialCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 255 °C | 446 - 491 °F | Injection Molding |
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 255 °C | 446 - 491 °F | Injection Molding |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® DP1000DU PBT Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3250M PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG5150 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good SurfaceApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG5152 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good Surface, High ImpactApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG5300 PBT+PET+GF30% Description: Injection Molding, PBT+PET+GF30%, Good Surface Application: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Start Point: 245°C |
Kingfa PET-G15 15% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Start Point: 245°C |
Kingfa PET-G30 30% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Start Point: 245°C |
Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Rear Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 240 - 255 °C | 464 - 491 °F | Injection Molding |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |