Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 300 - 320 °C | 572 - 608 °F | |
Unitika P-3001S Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |