Polymer Property : Rear Barrel Temperature = 325 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 163 - 185 °C
325 - 365 °F
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish..
Rear Barrel Temperature 163 - 188 °C
325 - 370 °F
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi..
Rear Barrel Temperature 163 - 188 °C
325 - 370 °F
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE)
Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R..
Rear Barrel Temperature 163 - 185 °C
325 - 365 °F
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE)
Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P..
Rear Barrel Temperature 163 - 188 °C
325 - 370 °F
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE)
Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan..
Rear Barrel Temperature 163 °C
325 °F
LyondellBasell Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade
ApplicationsPetrothene NA247000 provides a balance of stiffness and tear strength. Typical applications include tamper evident caps and closures.Regulatory StatusNA247000 meets the requirements of t..
Rear Barrel Temperature 163 °C
325 °F
DuPont Surlyn® 1702SBR  (discontinued **)
DuPont™ Surlyn® 1702SBR is a zinc-type resin made from ethylene/methacrylic acid copolymer. This resin has slip, antiblock, and chill roll release additives included in the resin to reduce the coe..