Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 177 - 216 °C | 351 - 421 °F | |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 421 °F | |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Rear Barrel Temperature | 210 - 216 °C | 410 - 421 °F | |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Rear Barrel Temperature | 210 - 216 °C | 410 - 421 °F | |
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer .. |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 421 °F | |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 421 °F | |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |