Polymer Property : Rear Barrel Temperature = 509 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 265 °C
482 - 509 °F
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Rear Barrel Temperature 245 - 265 °C
473 - 509 °F
Start Point: 250°C
Kingfa JE2-R2G20 Glass Fiber Reinforced ABS/PBT Alloy
Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a..
Rear Barrel Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity
Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical
Rear Barrel Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity
Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical
Rear Barrel Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical LUMID GP1300A(W) PA6, High Viscosity
Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical
Rear Barrel Temperature 245 - 265 °C
473 - 509 °F
Injection Molding
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Rear Barrel Temperature 240 - 265 °C
464 - 509 °F
Injection Molding
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
Rear Barrel Temperature 230 - 265 °C
446 - 509 °F
Injection Molding
LG Chemical LUPOY HI5002A PC/ABS, High Impact
Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Rear Barrel Temperature 255 - 265 °C
491 - 509 °F
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry
Information provided by Unitika Ltd.
Rear Barrel Temperature 255 - 265 °C
491 - 509 °F
Unitika A3130 PA6, 35% Mineral Reinforced, Dry
Information provided by Unitika Ltd.
Rear Barrel Temperature 220 - 265 °C
428 - 509 °F
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin
Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 220 - 265 °C
428 - 509 °F
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin
Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 220 - 265 °C
428 - 509 °F
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 245 - 265 °C
473 - 509 °F
Start Point: 250°C
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy
Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a..
Rear Barrel Temperature 245 - 265 °C
473 - 509 °F
Injection Molding
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage
Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical