Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:..
Rear Barrel Temperature 316 - 330 °C
601 - 626 °F
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)  (discontinued **)
Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)  (Unverified Data**)
Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber
Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient..
Rear Barrel Temperature 316 - 321 °C
601 - 610 °F
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Rear Barrel Temperature 316 - 321 °C
601 - 610 °F
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber
Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Rear Barrel Temperature 316 - 330 °C
601 - 626 °F
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep ..
Rear Barrel Temperature 316 - 330 °C
601 - 626 °F
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep ..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber
Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Conditioned)
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry)
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; ..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber
Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber
Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn..
Rear Barrel Temperature 316 - 321 °C
601 - 610 °F
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel resin. This grade was developed for autom..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)  (Unverified Data**)
Amodel DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of ..
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers.
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers.
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry  (discontinued **)
Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..