Polymer Property : Drying Temperature = 177 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 165 - 177 °C

@Time 14400 sec
329 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber  (discontinued **)
RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 ..
Drying Temperature 149 - 177 °C

@Time 14400 sec
300 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU)
Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn..
Drying Temperature 166 - 177 °C

@Time 14400 sec
331 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7535 Polyphenylsulfone (PPSU)
Radel® R-7535 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu..
Drying Temperature 166 - 177 °C

@Time 14400 sec
331 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU)
Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu..
Drying Temperature 166 - 177 °C

@Time 14400 sec
331 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU)
Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product ..
Drying Temperature 149 - 177 °C

@Time 9000 - 14400 sec
300 - 351 °F

@Time 2.50 - 4.00 hour
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Drying Temperature 149 - 177 °C

@Time 9000 - 14400 sec
300 - 351 °F

@Time 2.50 - 4.00 hour
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Drying Temperature 149 - 177 °C

@Time 9000 - 14400 sec
300 - 351 °F

@Time 2.50 - 4.00 hour
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber
Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Drying Temperature 149 - 177 °C

@Time 9000 - 14400 sec
300 - 351 °F

@Time 2.50 - 4.00 hour
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU), 30% Glass Fiber
Veradel® AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Drying Temperature 149 - 177 °C
300 - 351 °F
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..
Drying Temperature 149 - 177 °C
300 - 351 °F
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)  (Unverified Data**)
Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..
Drying Temperature 149 - 177 °C
300 - 351 °F
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU)  (Unverified Data**)
Veradel AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..