Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
PTS Trilac® ABS-RC3000 Recycled Black ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 °C | 190 °F | max 6 hours |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 °C | 190 °F | |
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Drying Temperature | 87.8 °C | 190 °F | |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Drying Temperature | 88.0 °C @Time 14400 sec |
190 °F @Time 4.00 hour |
|
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Drying Temperature | 90 - 100 °C | 190 - 212 °F | |
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Drying Temperature | 88.0 °C @Time 7200 - 14400 sec |
190 °F @Time 2.00 - 4.00 hour |
|
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Drying Temperature | 87.8 - 110 °C | 190 - 230 °F | |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Drying Temperature | 88.0 °C @Time 7200 - 14400 sec |
190 °F @Time 2.00 - 4.00 hour |
|
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Drying Temperature | 87.8 - 110 °C | 190 - 230 °F | |
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
TPI Porene® ABS-SP-100 Super High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | air dew point <-40°C |
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | air dew point <-40°C |
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | air dew point <-40°C |
Lubrizol Estane® 2355-95AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Fuel resistant, extrusion laminate coatingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Dow Chemical.Lubrizol acquired the Pellethane.. |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | Air dew point <-40°C |
Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan EX401 Copolyester Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan MX731 Copolyester Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan TX1501HF Copolyester Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan TX2000 Copolyester Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | air dew point <-40°C |
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod.. |
|||
Drying Temperature | 87.8 - 104 °C | 190 - 220 °F | air dew point <-40°C |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |