Processing Properties Metric English Comments
Drying Temperature 150 - 160 °C
302 - 320 °F
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU)
Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne
Drying Temperature 150 - 160 °C
302 - 320 °F
Eastman 7352 PET  (discontinued **)
VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73..
Drying Temperature 135 - 160 °C
275 - 320 °F
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Drying Temperature 150 - 160 °C
302 - 320 °F
Eastman Eastar EN010 Copolyester
Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers
Drying Temperature 150 - 160 °C
302 - 320 °F
Eastman Eastar EN052 Polyester
Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
Drying Temperature 150 - 160 °C
302 - 320 °F
Eastman Eastar EN063 Polyester
Eastar Polyester EN063 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Eastar Polyester EN063 is a homopolymer ..
Drying Temperature 150 - 160 °C
302 - 320 °F
Eastman Eastar EN067 Copolyester, Natural
Eastar Copolyester EN067 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability characteristics. Due to slower crystallization kinetics, t..
Drying Temperature 150 - 160 °C
302 - 320 °F
Eastman Eastar MN021 Copolyester
Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
Drying Temperature 150 - 160 °C
302 - 320 °F
Eastman Eastar MN052 Polyester, Natural
Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..