Polymer Property : Drying Temperature = 65.6 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black
Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey
Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 51.7 - 65.6 °C
125 - 150 °F
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 48.9 - 65.6 °C
120 - 150 °F
PolyOne Lubri-Tech™ SY-000/10T-2S Natural Polystyrene (PS), PTFE Lubricated  (discontinued **)
Description/Features:High ImpactPTFE LubricatedInformation provided by PolyOne Corporation.
Drying Temperature 48.9 - 65.6 °C
120 - 150 °F
Usually not required
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Drying Temperature 48.9 - 65.6 °C
120 - 150 °F
Usually not required
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Drying Temperature 48.9 - 65.6 °C
120 - 150 °F
Usually not required
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol..
Drying Temperature 48.9 - 65.6 °C
120 - 150 °F
Usually not required
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black
For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add..