Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber
(discontinued **) A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 253-36 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours if desired. |
ExxonMobil Santoprene® 8211-45W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-55 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-75 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 10800 - 14400 sec |
180 - 199 °F @Time 3.00 - 4.00 hour |
|
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 - 10800 sec |
180 - 199 °F @Time 2.00 - 3.00 hour |
|
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Drying Temperature | 82.0 - 104 °C | 180 - 219 °F | |
Spartech PP5140 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew pint <-40°C |
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Drying Temperature | 82.0 °C | 180 °F | |
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 °C | 180 °F | |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 °C | 180 °F | |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Trefsin® 3101-65 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |