Polymer Property : Drying Temperature = 95.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-7712/GY PP-copolymer, with carbon fiber and glass fiber, electrically conducting
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber
Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-8347/RD PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-8452-1 PP-copolymer, with aramid reinforcement, lubricant modified
Applications: Office communication.Low warpage, isotropic shrinkage characteristics.Dynamic stressed parts.Information provided by Lehmann & Voss & Co.KG
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-8452-2 PP-copolymer, with carbon fiber, aramid reinforcement, lubricant modified
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Information provided by..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced
Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Injection Molding
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Injection Molding
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Injection Molding
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Injection Molding
LG Chemical LUPOY GP5100 PC/ABS+GF10%
Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by..
Drying Temperature 85.0 - 95.0 °C

@Time 7200 - 18000 sec
185 - 203 °F

@Time 2.00 - 5.00 hour
IRPC Polimaxx Porene KU200 Acrylonitrile Butadiene Styrene
Applications:extrusion applicationautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances
Drying Temperature 85.0 - 95.0 °C

@Time 7200 - 18000 sec
185 - 203 °F

@Time 2.00 - 5.00 hour
IRPC Polimaxx Porene KU650 Acrylonitrile Butadiene Styrene
Applications:injection moldingautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Kostat BK-STAT 7048BK ABS Compound
BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Kostat BK-STAT 7048BK ABS Sheet
BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness ..
Drying Temperature 80.0 - 95.0 °C
176 - 203 °F
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Drying Temperature 70.0 - 95.0 °C
158 - 203 °F
Average value: 81.2 °C Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Pre-drying
Styrolution Luran® S KR 2867 C WU Colored ASA+PC
Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO..