Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 0.330 hour @Temperature 25.0 °C |
0.330 hour @Temperature 77.0 °F |
ASTM D711 |
Lotus Nano Paint NAP 101 Nano-paint Description: Traffic marking nano-paints improved with nano-particles to get better performance in traffics on the road. Better mechanical properties, excellent traffic performance and more durabili.. |
|||
Dry Time | 0.330 hour @Temperature 25.0 °C |
0.330 hour @Temperature 77.0 °F |
ASTM D711 |
Lotus Nano Paint NAP 102 Nano-paint Description: This grade has resistance in affecting pollutions on surface of paint and cause that traffic lots be clean and do better performance. This paint is suitable for places with high polluti.. |
|||
Dry Time | 0.330 hour @Temperature 25.0 °C |
0.330 hour @Temperature 77.0 °F |
ASTM D711 |
Lotus Nano Paint NAP 103 Nano-paint Description: This product has more resistance in environment and surface temperature and cause to be more durable on the road. For tropical places this paint cause better traffic lots in long time.A.. |
|||
Dry Time | 0.330 hour @Temperature 25.0 °C |
0.330 hour @Temperature 77.0 °F |
ASTM D711 |
Lotus Nano Paint NAX 01 Tow-Component Nano-paint Description: More durable and specific application methods. This paint is suitable for traffic signs on the road, cross-walks, warning vibrating lines and limited lot marking. Related machines could.. |
|||
Dry Time | 0.330 hour @Temperature 25.0 °C |
0.330 hour @Temperature 77.0 °F |
ASTM D711 |
Lotus Nano Paint NAX 01P Tow-Component Nano-paint Description: More durable and specific application methods. This paint is suitable for traffic signs on the road, cross-walks, warning vibrating lines and limited lot marking. Related machines could.. |