Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor.. |
|||
Dry Time | 1.00 hour | 1.00 hour | |
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C). |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |