Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2 - 4 hour | 2 - 4 hour | No venting in an air circulating oven |
Polimeri Europa Sinkral® B 432/E ABS Resin Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in fresh-air dryer |
Polykemi AB POLYabs N20 ABS Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYasa 3010F Extra High Flow ASA Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PP EQX10030R UV Polypropylene, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 hour | 2 hour | |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in fresh-air dryer |
Polykemi AB POLYabs HD2 ABS Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPC GF15030 PD2 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Dry Time | 2 hour | 2 hour | |
PolyOne Edgetek® ATH-10CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Dry Time | 2 - 6 hour | 2 - 6 hour | |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Dry Time | 2 - 3 hour | 2 - 3 hour | |
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Multibase Multi-Flex® D 3604 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Pre-drying |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Diamond Polymers ABS 1000 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Dry Time | 2 - 16.0 hour | 2 - 16.0 hour | |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Dry Time | 2 - 16.0 hour | 2 - 16.0 hour | |
Akro-Plastic Akromid® T6 GF30 (3501) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
BASF Ultramid® 8351 HS BK 106 PA6 (Dry) Description: Ultramid 8351 HS BK-106 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
Dry Time | 2 - 16.0 hour | 2 - 16.0 hour | |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Option 3 |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant Information provided by Polykemi AB |