Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-HS4000 General Purpose ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-HS7500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-RC3000 Recycled Black ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin
(Unverified Data**) Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 24 hour | 2 - 24 hour | |
TPI Porene® ABS-SP-100 Super High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 16 - 24 hour | 16 - 24 hour | Demold time, catalyzed with QM CAT BLUE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Dry Time | 16 - 24 hour | 16 - 24 hour | Demold time, catalyzed with QM CAT BLUE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Dry Time | 16 - 24 hour | 16 - 24 hour | Demold time, catalyzed with QM CAT BLUE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Dry Time | 16 - 24 hour | 16 - 24 hour | Demold time, catalyzed with QM CAT SKIN 30 |
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l.. |
|||
Dry Time | 16 - 24 hour | 16 - 24 hour | Demold time, catalyzed with QM CAT BLUE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Dry Time | 1 - 24 hour | 1 - 24 hour | Recoat |
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15.. |
|||
Dry Time | 1 - 24 hour | 1 - 24 hour | Recoat |
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F. |
|||
Dry Time | 1 - 24 hour | 1 - 24 hour | Recoat |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Dry Time | 1 - 24 hour | 1 - 24 hour | Recoat |
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F. |
|||
Dry Time | 1 - 24 hour | 1 - 24 hour | Recoat |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Dry Time | 16 - 24 hour | 16 - 24 hour | Demold time, catalyzed with QM CAT BLUE |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |