Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 8.00 - 12.0 hour | 8.00 - 12.0 hour | |
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Dry Time | 8.00 - 12.0 hour | 8.00 - 12.0 hour | |
PolyOne OnForce™ LFT UR-40 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Dry Time | 8.00 - 12.0 hour | 8.00 - 12.0 hour | |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Dry Time | 8.00 - 12.0 hour | 8.00 - 12.0 hour | |
PolyOne OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Dry Time | 8.00 - 24.0 hour | 8.00 - 24.0 hour | |
Unitika FUN-8000 Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd. |
|||
Dry Time | 8.00 - 10.0 hour | 8.00 - 10.0 hour | Demold time, catalyzed with Moldmaster Green |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Dry Time | 8.00 - 10.0 hour | 8.00 - 10.0 hour | Demold time, catalyzed with Moldmaster Green |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Dry Time | 8.00 hour | 8.00 hour | Handling |
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C). |