Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYabs S20 ABS
Information provided by Polykemi AB |
Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYfill PP CPX10030 UV Polypropylene, Mineral Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB |
Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PP HIP15025 HC Polypropylene
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYfill PPC TS6020 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GF1020 Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH DGF101015 PB Polypropylene Homopolymer, Glass Fibre/Mineral, Chemically Coupled
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GF12030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GF5020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GK8040 Polypropylene Homopolymer, Glass Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH TS15040 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB |
Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYabs F20 ABS
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH BK901010 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH GF8030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH T15020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
Mold Pressure |
Beijing Chemical Industry KAIFA® GL2200 ABS Good Flow Grade
High impact, Easy processingInformation provided by Beijing Chemical Industry Research Institute (Group) |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
Mold Pressure |
Beijing Chemical Industry KAIFA® GL3200 ABS Flame-Retardant Grade
Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
Mold Pressure |
Beijing Chemical Industry KAIFA® GL5200 ABS Extrusion Grade
Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group) |
Back Pressure |
1.00 - 1.50 MPa |
145 - 218 psi |
|
Polykemi AB POLYabs F20 GF17 ABS, Glass Fiber Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH TS8038 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPHC EP1001F Polypropylene
Information provided by Polykemi AB |
Back Pressure |
1.00 - 2.00 MPa |
145 - 290 psi |
|
Polykemi AB POLYfill PPH TS2040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |