Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AX-1500W Conditioned Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AXF-1500-05 Conditioned Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AXG-1500-300 Conditioned Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika C300VN Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika LM-8503-10 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika P-1001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika P-3001S Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika U-8400H U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika FUN-8000 Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika L-8005 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA) Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-7307 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika UM-8430RG Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika U-8000 U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |