Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 20 - 50 rpm | 20 - 50 rpm | |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Screw Speed | 20 - 80 rpm | 20 - 80 rpm | |
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Screw Speed | 20 - 80 rpm | 20 - 80 rpm | |
Huntsman AVALON® 85 ABX Thermoplastic Polyurethane Introduction: AVALON 85 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Screw Speed | 20 - 80 rpm | 20 - 80 rpm | |
Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
Screw Speed | 20 - 80 rpm | 20 - 80 rpm | |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Screw Speed | 20 - 50 rpm | 20 - 50 rpm | |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant PCSP0014 GREY Polycarbonate, Stainless Steel Fiber, EMI Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 6001 GP HSL Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 6001 HV HSL Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA211 Nylon 6, General Purpose Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA213G50 Nylon 6, 50% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PBTSP0006 Polyester Elastomer Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PCSP0011 Polycarbonate Alloy, Glass Fiber and Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol TES3050A Thermoplastic Elastomer Alloy Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |