Processing Properties Metric English Comments
Screw Speed 40 - 80 rpm
40 - 80 rpm
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Triloy® 410N PC/PET alloy, Flame Retardant  (discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
Screw Speed 50 - 80 rpm
50 - 80 rpm
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 40 - 80 rpm
40 - 80 rpm
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Screw Speed 40 - 80 rpm
40 - 80 rpm
Extrusion
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Screw Speed 40 - 80 rpm
40 - 80 rpm
Injection Molding
LG Chemical LUCON PN9008 PPS+MF+GF
Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212..
Screw Speed 40 - 80 rpm
40 - 80 rpm
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Screw Speed 40 - 80 rpm
40 - 80 rpm
Gromax 1140LH TPE
Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject..
Screw Speed 40 - 80 rpm
40 - 80 rpm
Gromax 1155LL TPE
1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex..
Screw Speed 40 - 80 rpm
40 - 80 rpm
Gromax 1163LL TPE
163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext..
Screw Speed 20 - 80 rpm
20 - 80 rpm
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane
Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,..
Screw Speed 20 - 80 rpm
20 - 80 rpm
Huntsman AVALON® 65 AC Thermoplastic Polyurethane
Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia..
Screw Speed 20 - 80 rpm
20 - 80 rpm
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma..
Screw Speed 20 - 80 rpm
20 - 80 rpm
Huntsman AVALON® 85 AB Thermoplastic Polyurethane
Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma..
Screw Speed 20 - 80 rpm
20 - 80 rpm
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane
Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Triloy® 170 PC/PBT alloy
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Triloy® 210 PC/ABS alloy
Characteristics:Impact resistantHeat resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grillA..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Triloy® 230NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Trirex® 3027IR Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Trirex® 3025A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Screw Speed 40 - 80 rpm
40 - 80 rpm
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Screw Speed 40 - 80 rpm
40 - 80 rpm
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Conditioned)
Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio..
Screw Speed 40 - 80 rpm
40 - 80 rpm
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry)
Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o..
Screw Speed 20 - 80 rpm
20 - 80 rpm
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane
Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Triloy® 200 PC/ABS alloy
General purposeCharacteristics:Impact resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grill..