Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.917 - 1.08 min | 0.0153 - 0.0181 hour | per mm |
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Cure Time | 0.917 - 1.08 min | 0.0153 - 0.0181 hour | per mm |
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Cure Time | 0.917 - 1.33 min | 0.0153 - 0.0222 hour | per mm |
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo.. |