Polymer Property : Cure Time = 10.0 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 600 min
10.0 hour
Lord Adhesives 410 Flexible, High Impact and Peel Resistance, Long Working Time Acrylic Adhesive
Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e..
Cure Time 600 min
10.0 hour
2 hrs @ 65°C + 8 hrs @ 115°C
Tra-Con Tra-Bond 2208 Water White High Temperature Epoxy Adhesive
TRA-BOND 2208 is a clear, almost water-white low viscosity epoxy adhesive system recommended for rigid laminating, filament winding, potting and bonding applications. This all-liquid formulation con..
Cure Time 600 min

@Temperature 82.2 °C
10.0 hour

@Temperature 180 °F
Zyvex Performance Materials Arovex™ 180 Carbon Nanotube Strengthened Prepreg
Arovex® 180 Prepreg is a 180°F (82°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Arovex 180 resin contains an optimum level of carbon nanotub..
Cure Time 600 min
10.0 hour
2 hrs @ 65°C + 8 hrs @ 115°C
Tra-Con Tra-Cast 3357 High Temperature Rigid Epoxy Casting System
TRA-CAST 3357 is a smooth pouring, low viscosity casting resin system recommended for rigid, large mass potting, encapsulating, laminating, filament-winding and coil embedment applications where the..
Cure Time 600 min
10.0 hour
2 hrs @ 65°C + 8 hrs @ 115°C
Tra-Con Tra-Bond 2202 Low Viscosity/High Temperature Epoxy Adhesive
TRA-BOND 2202 is a low viscosity, high temperature cure epoxy resin system developed for rigid laminating, filament winding, potting and bonding applications where a clear, almost transparent adhesi..
Cure Time 600 min
10.0 hour
Tack-Free Time
3M AC-215 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa..
Cure Time 600 min
10.0 hour
3M AC-240 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan..
Cure Time 600 min
10.0 hour
Time to Handling Strength
3M Scotch-Weld™ EC2216 Structural Adhesive
High Performance, Very flexible bondsInformation provided by 3M
Cure Time 600 min
10.0 hour
Time to Handling Strength
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..