Polymer Property : Cure Time = 720 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 480 - 720 min

@Temperature 23.0 °C
8.00 - 12.0 hour

@Temperature 73.4 °F
Master Bond Mastersil 711 Fast Curing One Component Silicone
MasterSil 711 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This specialty product features an exceptional..
Cure Time 480 - 720 min

@Temperature 23.0 °C
8.00 - 12.0 hour

@Temperature 73.4 °F
Master Bond EP30-4 Fast Curing Non-Yellowing Two Component Epoxy System
Master Bond Polymer Adhesive EP30-4 is a unique low viscosity, two component epoxy adhesive for bonding, coating, and sealing formulated to cure at room temperature or more rapidly at elevated tempe..
Cure Time 60.0 - 720 min
1.00 - 12.0 hour
Full Cure; Unprimed
Loctite® Gasket Eliminator® 515 Flange Sealant
Anaerobic GasketingLoctite® 515 Flexible Cure Gasket Eliminator® Flange SealantMakes flexible gaskets for rigid machined flanges with less than 0.050" gap. Flexes with flanges that move in servic..
Cure Time 60.0 - 720 min

@Temperature 80.0 - 150 °C
1.00 - 12.0 hour

@Temperature 176 - 302 °F
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste
BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical..
Cure Time 60.0 - 720 min

@Temperature 80.0 - 150 °C
1.00 - 12.0 hour

@Temperature 176 - 302 °F
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid
Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin..
Cure Time 60.0 - 720 min

@Temperature 80.0 - 150 °C
1.00 - 12.0 hour

@Temperature 176 - 302 °F
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste
Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris..
Cure Time 60.0 - 720 min

@Temperature 80.0 - 150 °C
1.00 - 12.0 hour

@Temperature 176 - 302 °F
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste
Metalfix-PH™ is MetalFix-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Cha..
Cure Time 480 - 720 min
8.00 - 12.0 hour
Tack Free Time, catalyzed with QM CAT SKIN 30
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material
QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l..
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
BCC Products BC 6004 Epoxy Surface Coat
BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi..
Cure Time 480 - 720 min
8.00 - 12.0 hour
Time to Handling Strength
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M
Cure Time 480 - 720 min
8.00 - 12.0 hour
Time to Handling Strength
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Cure Time 60.0 - 720 min

@Temperature 80.0 - 150 °C
1.00 - 12.0 hour

@Temperature 176 - 302 °F
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid
Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin..
Cure Time 60.0 - 720 min

@Temperature 80.0 - 150 °C
1.00 - 12.0 hour

@Temperature 176 - 302 °F
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste
SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra..
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
BCC Products BC 5008-2 General Purpose Epoxy System
BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A..
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
BCC Products BC 6005 Epoxy Surface Coat
BC 6005 is a snow white thixotropic epoxy resin designed specifically for quality reproduction of a variety of surfaces. A room temperature cure system that offers ample working time yet affords qui..
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
demold time
BCC Products DP-11-88 Urethane Adhesive
DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions ..
Cure Time 480 - 720 min
8.00 - 12.0 hour
Time to Handling Strength
3M Scotch-Weld™ 2158 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2158 B/A is a gray, two-part, high strength adhesive that chemically cures at room temperature. It has good adhesion to a variety of substrates including metals, ma..
Cure Time 60.0 - 720 min
1.00 - 12.0 hour
Full Cure, Unprimed
Loctite® 574 Semi-rigid Cure Anaerobic Sealant
Anaerobic GasketingLoctite® 574 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Fast curing, large gaps
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
BCC Products BC 5010 Epoxy Laminating System
BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor..
Cure Time 30.0 - 720 min

@Temperature 45.0 - 150 °C
0.500 - 12.0 hour

@Temperature 113 - 302 °F
Average value: 284 min Grade Count:11
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..
Cure Time 480 - 720 min
8.00 - 12.0 hour
Time to Handling Strength
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..