Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 360 - 960 min @Temperature 23.0 °C |
6.00 - 16.0 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond LH054 Anaerobic Threadsealant Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta.. |
|||
Cure Time | 480 - 960 min | 8.00 - 16.0 hour | |
Lord Adhesives 312 General Purpose, Low Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 480 - 960 min | 8.00 - 16.0 hour | |
Lord Adhesives 3170 Two-component, high cold strength, cryogenic application Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 720 - 960 min | 12.0 - 16.0 hour | |
Trelleborg Emerson & Cuming Stycast® 1497 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Cure Time | 720 - 960 min @Temperature 24.0 °C |
12.0 - 16.0 hour @Temperature 75.2 °F |
|
BCC Products BC 6060 Epoxy Surface Coat/Casting BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum.. |
|||
Cure Time | 720 - 960 min | 12.0 - 16.0 hour | Time to Handling Strength |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Cure Time | 1.60 - 960 min @Temperature 68.3 - 204 °C |
0.0267 - 16.0 hour @Temperature 155 - 400 °F |
Average value: 31.0 min Grade Count:407 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |