Polymer Property : Dew Point = -25.0 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dew Point -31.7 °C
-25.0 °F
Average value: -31.7 °C Grade Count:22
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Dew Point -31.7 °C
-25.0 °F
Average value: -31.7 °C Grade Count:10
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Dew Point -31.7 - -28.9 °C
-25.0 - -20.0 °F
Average value: -29.8 °C Grade Count:3
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..