Processing Properties | Metric | English | Comments |
---|---|---|---|
Dew Point | -31.7 - -28.9 °C | -25.0 - -20.0 °F | Average value: -30.7 °C Grade Count:17 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Dew Point | -31.7 °C | -25.0 °F | Average value: -31.7 °C Grade Count:19 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |