Polymer Property : Shelf Life = 1.50 Month Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Shelf Life 1.50 Month
1.50 Month
(45 days) at 43°C, clear melt without filtration
Dow ISONATE™ 125M Pure MDI
ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers f..
Shelf Life 1.50 Month
1.50 Month
(45 days) at 43°C, clear melt without filtration
Dow ISONATE™ 125MDR Pure MDI
ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers ..
Shelf Life 1.50 Month
1.50 Month
27-30°C
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni..
Shelf Life 1.50 Month
1.50 Month
27-30°C
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication ..