Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 9.00 Month | 9.00 Month | @ 70°F |
Parker Chomerics CHO-SHIELD® 4904 Conductive Coating Conductive Nickel-Filled Acrylic Coating. This is the lowest coast in the family of nickel-filled, electrically conductive acrylic coatings. CHO-SHIELD® 4904 is resistant to solvent attack and to f.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Parker Chomerics CHO-SHIELD® 611 Part A Conductive Coating Comments: Variant of CHO-SHIELD 596Typical Applications:Protecting EMI flangesInformation provided by Chomerics |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Parker Chomerics Tecknit® 0236 Conductive Silicone Sealant/Adhesive Comments: Thick flexible pasteTypical Applications: Bonding Ag/Al elastomerInformation provided by Chomerics |
|||
Shelf Life | 9.00 Month | 9.00 Month | Unopened Container |
Parker Chomerics Tecknit TeckBond™-NC Nickel Coated Graphite-Filled Adhesive Description: TECKBOND-NC is a silicone rubber base filled with nickel coated graphite particles to produce a highly conductive one-component adhesive sealant. The system is an RTV moisture-cured com.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | unopened |
Parker Chomerics CHO-BOND 2165 Polyurethane Sealant Conductive sealant is a stabilized copper filled, two component polyurethane. It has excellent electrical and physical properties for aerospace and military applications. CHO-BOND® 2165 sealant is .. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Parker Chomerics CHO-BOND 360-20 Conductive Epoxy Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E.. |
|||
Shelf Life | 9.00 Month @Temperature 25.0 °C |
9.00 Month @Temperature 77.0 °F |
|
Lord Adhesives Thermosetâ„¢ SC-303 Silicone Encapsulant, Flame Retardant Lord SC-303 is a two component silicone elastomer that provides excellent thermal conductivity, while retaining the other desirable properties associated with silicones. It is a low viscosity, easil.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Lucite International Series 100 Liquid Acrylic Resin LUCITE® LIQUID ACRYLIC RESINS SERIES 100For the manufacture of solid surface shapesAmbient temperature cureCan be used on batch or continuous in-line mixing equipmentInformation provided by Lucit.. |
|||
Shelf Life | 9.00 Month @Temperature 5.00 - 10.0 °C |
9.00 Month @Temperature 41.0 - 50.0 °F |
in unopened original container |
Heraeus Cleviosâ„¢ P VP AI 4083 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP AI 4083 is an antistatic material based o.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Sika Industry SikaTack UltraFast Fast Cure One Part Polyurethane Adhesive Sika UltraFast SikaTack Fast Cure One Part Polyurethane AdhesiveThis revolutionary product uses heat instead of moisture to "pre-cure" the adhesive. The product is heated before applications using a.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Solvay REPEL-O-TEX® CRYSTAL Surfactant Description: Designed for liquid laundry formulations to impart soil release properties to polyester fabrics, offering protection against adhesion of greasy soils between wash cycles.Chemical Name: .. |
|||
Shelf Life | 9.00 Month | 9.00 Month | shelf life at 5ºC |
Loctite® 3873 1 component acrylic High Conductivity Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Dow Corning SE 4422 SILICONE RTV One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning |
|||
Shelf Life | <= 9.00 Month | <= 9.00 Month | |
Abatron AboWeld 8708-7 One-Component Structural/Dielectric Epoxy AboWeld 8708-7 is a highly filled, class H (180°C) structural, heat-conductive adhesive paste for FASTER high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulatin.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-236 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-350 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-350 Class C-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-350 Class C-8(24) Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-645 B-2 Aerospace Sealant 3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filli.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-665 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-665 Class B are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-730 Class B-12 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-736 B-2 Aerospace Sealant 3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an .. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-370 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-370 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Shelf Life | 9.00 - 12.0 Month | 9.00 - 12.0 Month | |
3M Scotch-Seal™ 1252 Tamper Proof Sealant 3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustme.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-350 Class B-1/4 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Solvay RHODAPEX® EST-30/BLB Surfactant Chemical Name: Sodium Trideceth(3) SulfateCAS: 25446-78-0Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX EST-30/BLB is an APE-Free emulsifier for acrylic, .. |
|||
Shelf Life | 9.00 Month | 9.00 Month | |
Lucite International Series 500 Liquid Acrylic Resin LUCITE® LIQUID ACRYLIC RESINS SERIES 500For the manufacture of solid surface sheet & worktopsAmbient temperature curing resin with low VOC emissionsCan be used on batch or continuous in-line mixing.. |
|||
Shelf Life | 9.00 Month @Temperature <=26.7 °C |
9.00 Month @Temperature <=80.1 °F |
|
3M AC-236 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Shelf Life | 9.00 Month | 9.00 Month | shelf life at 5ºC |
Loctite® Output™ 383 Acrylic Adhesive Acrylic Bonding Adhesives and Thermally Conductive BondersLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impa.. |