Polymer Property : Gel Time = 1.50 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 0.500 - 1.50 min
0.500 - 1.50 min
Park Electrochemical Nelcote® P-670F Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670F is a versatile, non-styrenated/low VOC polyester resin. P670F is used in a wide variety of applications including tooling and aircraft structures.Key Features and Benefits:Non-styre..
Gel Time 0.500 - 1.50 min
0.500 - 1.50 min
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:..
Gel Time 1.00 - 1.50 min

@Temperature 171 °C
1.00 - 1.50 min

@Temperature 340 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Gel Time 1.00 - 1.50 min

@Temperature 171 °C
1.00 - 1.50 min

@Temperature 340 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Gel Time 1.00 - 1.50 min

@Temperature 171 °C
1.00 - 1.50 min

@Temperature 340 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Gel Time 1.00 - 1.50 min

@Temperature 171 °C
1.00 - 1.50 min

@Temperature 340 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 7781 E-Glass Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..