Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 12.0 - 22.0 min | 12.0 - 22.0 min | Prepreg |
Hexcel® HexPly® 8552 Epoxy Matrix, Carbon Fabric Form Information provided by HexCel |
|||
Gel Time | 12.0 - 22.0 min | 12.0 - 22.0 min | Prepreg |
Hexcel® HexPly® 8552 Epoxy Matrix, Carbon Tape Form Information provided by HexCel |