Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 175 - 220 °C | 347 - 428 °F | |
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a.. |
|||
Melt Temperature | 175 - 205 °C | 347 - 401 °F | |
Reliance Industries Relene B56003 Polyethylene Relene B56003 is a High Density Polyethylene grade suitable for general purpose extrusion blow molding applications. Articles blown from this grade exhibit good stiffness. The resin offers good me.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 13 wt% Methacrylic Acid.Nucrel® 1302 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process po.. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 199 °C Grade Count:6 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 195 °C Grade Count:22 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Melt Temperature | 175 - 238 °C | 347 - 460 °F | Degrades above 238°C. |
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including poly.. |
|||
Melt Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 13E71 POM Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided .. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 2 POM Polyoxymethylene (POM). Unfilled. High viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 23UV POM Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 23UVE71 POM Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 3E71 POM Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 9 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13-15T G/15 POM, 15% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13-20T POM, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latishield 73/13-07A POM, Steel Fiber Reinforced EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latistat 73/13-06 POM Dissipative product based on Polyoxymethylene (POM). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Melt Temperature | 175 - 205 °C | 347 - 401 °F | blown film extrusion |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melt Temperature | 175 - 205 °C | 347 - 401 °F | blown film extrusion |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | Extrusion Coating |
DuPont™ Elvax® 3175LGA Ethylene Vinyl Acetate DuPont™ Elvax® 3175LGA is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | Blown/Cast Film Coextrusion |
DuPont™ Elvax® 3190A Ethylene Vinyl Acetate DuPont™ Elvax® 3190A is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Melt Temperature | 175 °C | 347 °F | |
AdvanSource Biomaterials HYDROTHANE™ Hydrophilic Thermoplastic Polyurethane AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether aliphatic polyurethanes designed for use as coatings of catheters, sutures, intr.. |
|||
Melt Temperature | 175 - 230 °C | 347 - 446 °F | |
NOVA Chemicals Sclair® D916-39 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, high stiffness, superior strength, gel free, excellent UV resistance.Applications: Industrial woven bags, tarpaulins.Data provided by th.. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 194 °C Grade Count:62 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 198 °C Grade Count:27 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 175 - 315 °C | 347 - 599 °F | Average value: 220 °C Grade Count:9 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3175LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3175 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13 Y/20 POM, 20% Aramid Fiber Reinforced Self-lubricating product based on Polyoxymethylene (POM). Aramid fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |