Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Molding |
PolyOne Lubri-Tech™ AT-10GB/15KV Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledAramid Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 199 - 216 °C | 390 - 421 °F | Typical Extrusion |
LyondellBasell Alathon® L5045 High Density Polyethylene ApplicationsALATHON L 5045 is a medium molecular weight high density polymer for use in blown film extrusion applications. Typical applications include millinery bags, coextrusions and plastic nett.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | |
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Melt Temperature | 182 - 216 °C | 360 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Total 9458 HDPE Film Grade Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba.. |
|||
Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe.. |
|||
Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
Westlake Hifor LT74104 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74104 is a high strength linear low density polyethylene containing no slip or antiblock. It is designed for blown film applications and is well suited for consumer an.. |
|||
Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
Westlake Hifor SC74557 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc.. |
|||
Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
Westlake Hifor Xtreme SC74845 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74845 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and high antiblock. Films produced with this resi.. |
|||
Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
Westlake LF1040 Butene Linear Low Density Polyethylene Westlake LF1040 is a butene LLDPE resin with excellent mechanical and sealing properties. It can be used in stretch film and can liner applications, and is suitable for blending with LDPE in packagi.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Melt Temperature | 199 - 216 °C | 390 - 420 °F | Molding |
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Molding |
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 193 - 216 °C | 380 - 420 °F | Extrusion |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Melt Temperature | 204 - 216 °C | 400 - 420 °F | |
Westlake Hifor Xtreme SC74859 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74859 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and high processing aid.Application/U.. |